Dear sir, We are using your product CONPLAST 430 G8 .As we are in the starting face of our PPA-GMADA MOHALI project, the use of admixture in our mix design finalized as properties of mix has been shown to yours rep. at site of Chandigarh zone staff which was found satisfactory. As the fresh consignments revised at site from in last few days, Now it becomes matter of concern that, the initially mix was found ok but after 20-30mims of pouring/finishing it start bleeding. (even after making all trial & error adjustment, about MC, slump, w/c, admixture dosage) effect is being seen continuously. We request you to please check the admixture / formulation by your expertise. So that this problem can be shorted out. Immediately action from your head is required. Please do the needful. RKSharma